Clean out the crack of debris. I use a small piece of sandpaper to accomplish this task. I tape off the area so I do not make a mess of the gelcoat. Then I lay a bead of epoxy into the crack. I wait for it to cure then wetsand the bead until it is smooth. It must be warmer than 60 degrees to accomplish such a repair.